DIY - Finishing Techniques

Avoid applying many and/or thick coats of varnish

The appearance of cracks in the final film is one of the finishing flaws that scares everyone. Firstly because there is no other way to fix it than sanding it down to the wood and reworking the whole process - which scares the manufacturer - and secondly because the finishing materials are blamed, scaring the supplier of such materials. It should be known, however, that it is not always the lacquers' fault. Most often the cause is a thick coat of varnish, a thick film obtained from a single application or from too many coats applied on top of each other.

thick layer of lake
photo source: frets.com

In production there is always a rush to finish products, especially when it comes to finishing. It's practically the last stage and if there was time to fix things before, now you have to work fast. The customer needed the furniture yesterday, the truck is waiting and there are penalties and many such reasons that make everything get done in a hurry. As a result, even though it is recommended to apply 2-3 coats of primer, with drying and sanding in between, apply one coat only, as little diluted as possible to avoid spills. And so drying is slower and appears orange peel.

photo source: popularwoodworking.com

In general, the orange peel-looking primer film is not so disturbing because the effect can be removed by sanding. But, there are risks. You sand too much and, from overzealousness, you end up with wood again. That's okay, we varnish, is generally the reaction. And then you apply a coat of varnish, and another, and another, because varnish has a smaller body (resin) and covers less than primer. In the end, although one coat of varnish is recommended, 3-4 coats are applied to achieve the desired look.

The consequences?

  • Much higher cost because the varnish is more expensive than primer,
  • Weaker coverage because the lake is poorer in body,
  • Heavy sanding between coats of varnish because the varnish is made not to scratch, so it will resist sanding,
  • Too many coats of varnish can eventually lead to cracks in the film.
thick layer of lake
photo source: hamerfanclub.com

There is also the option of not applying several coats of varnish, but applying a "good" one, i.e. thick, because good is not good. Applying a very thick coat of varnish also has consequences:

  • The thinner does not completely come out of the film. When wrapping in plastic film the thinner, which continues to come out, stays on top, softens the film again and prints from the packaging appear,
  • Risk of the film having an orange peel appearance,
  • Tensions in the thick compact layer lead to cracks in the film.

Consequently, as I recommend in the title, avoid applying many coats of varnish or primer and not one very thick one. Of course the worst is to have many and thick ones. I told you in an article that you should always read the instructions on how to use the materials: the instructions for use written on the box in the case of DIY products or the product data sheets in the case of industrial products. It always says how many coats of the product are recommended. More layers means cracks in the film. It also says how much material is recommended to be applied to a layer. More can also lead to cracks.

thick layer of lake
photo source: woodweb.com

It is definitely better to apply several thin coats than one thick one. More means 2-4, depending on recommendations. A total film of 500 gsm and more is very likely to crack, and if applied to solid wood, it will certainly crack with dimensional changes due to moisture variation. In the case of solvent-based products, the addition of thinner to the application is very important because it stimulates drying and the material dries faster.

I hope I've managed to convince you that it's better to delay the customer another day or pay a one-day late penalty on the truck, than to have to re-finish or worse, have the furniture returned for refinishing.

About the author

Mihaela Radu

Mihaela Radu is a chemical engineer but has a great passion for wood. She has been working in the field for more than 20 years, wood finishing being what defined her during this period. She gained experience working in a research institute, in her own company, as well as in a multinational. She wants to continuously share her experience with those who have the same passion - and more.

9 comments

Add a comment

Leave a Reply to Mihaela Radu Cancel reply

This site uses Akismet to reduce spam. Learn how your comment data is processed.

  • Hello,

    I follow and appreciate your articles.

    I need some advice on painting the exterior woodwork. The pine wood joinery is painted by the manufacturer with a coloured, water-based varnish, the initial finish being semi-gloss, fitted 10 years ago. For the first 3 years we protected the outside exposed part with a wax based product which was very effective. Due to carelessness, I discontinued this treatment, and now on the side exposed to the sun the "paint" has started to crack and I decided to redo the finish.
    I started cleaning the mobile window (dismantled) by scraping and sanding. I used three grits, 60/120/240. I used a water-based impregnator (two coats) and a thick tinted polish from Trilak. I applied the varnish with a sponge roller in very thin layers. The manufacturer specifies a certain amount of polish per square metre, I applied four coats with intermediate sanding (sponge 180). The colour is uniform but I am not happy with the appearance, it is very little glossy and the wood grain was not fully covered (appears raised) although I checked the surface after sanding and it looked ok. I also continued on the fixed window and on the holsters, and had an unpleasant surprise. I finished and impregnated similarly, still four coats of lacquer, but I may have given a thicker coat due to painting "in place" and wanting to cover the wood grain better, so the shade came out darker than on the movable window. The bigger problem is that when I peeled off the tape that protected the glass I also peeled the lacquer off the wood. I noticed that the lacquer didn't "catch" on the wood... Once again I think I gave the layers too bare, the embossed look of the fibre remained. Where did I go wrong, and what to do next? Should I apply less coats?
    I was happy with Trilak's thick lacquer, applied with a brush on the shutters (two coats), it came out almost fine, glossy looking, but there were fine streaks left from the brush... so I tried it now with the sponge roller. It has good UV resistance, the shutters have been painted for three years, no other care, they sit in the sun and are ok.

    Thanks in advance.

    • Good morning,
      The last sanding of the wood in white was too fine (240) and the wood could not absorb the thick lacquer. Hence the lack of adhesion. However, the sanding of the varnish was too small (180), which resulted in the removal of part of the layer and the final result was a thinner layer with less coverage.
      I recommend 150 grit as the last sanding of white wood, and at least 240 grit for sanding between layers.
      To increase the adhesion of the first coat of varnish you can thin it a little. Instead of water, you can use the coloured impregnating agent given as a first coat to prevent the wood fibre from lifting too much. This is if the varnish is also water soluble (that's how I figured it out). The dilution should not exceed 10%. As far as I can tell the product is thixotropic (the traces left behind by the brush) and if you add more water you lose this property, the product becomes very fluid, and there is a risk of spillage.
      Lack of gloss can be from very thin coats, coarse sanding between coats, but also from varnish - it has low gloss. That's how you bought it, or you didn't mix it well and the matting agent settled to the bottom of the can. So you have different gloss levels from coat to coat, the first being the most glossy and the last, visible, the most matt. You must mix the product well in the packaging before application. Use a rod, stick, or something similar. This way the mixing will be more efficient than simply suturing the can.
      I hope I've been useful.
      All the best.

  • Hello,
    I have a round wood house and I am going to apply the varnish coats. Can you tell me what kind of varnish to buy and how to apply it? Possibly what brand of product to look for.

  • I kiss my hands,
    I read with great interest your articles and would need your help and guidance for finishing some air purifiers whose housings will be made entirely of solid laminated milled & cnc engraved basswood. How can I get in touch with you?
    Yours faithfully
    Silviu Măgureanu
    AJA Registrars Romania
    http://www.ajaromania.net

  • Hello,
    I want to install pine floor in my house (the plank is about 3 cm) and I would like to ask you what materials I should use (wood stain, varnish stain, primer, varnish,...etc.) and in what order/if any and which layers should be sanded (I would like to specify that I would like to slightly darken the color of the wood and I would like to protect it from scratches and cleaning solutions). Another question would be if the wood should be treated with any solution on the underside as well (against mould or decay).
    I inquired at some DIY stores and at a warehouse specializing in wood maintenance/finishing solutions and it seemed to me that everyone was trying to sell the products without fully advising you (nowhere was I told that a very important difference between water-based and solvent-based lacquer/primer, except for price, is that the former lasts longer over time-so it justifies the higher price). For example, I've been told that I can just apply two coats of primer without applying traffic varnish because it's no longer necessary (from what I've read in one of your articles primer doesn't have the same properties as varnish), that it's not necessary to apply multiple coats of primer/varnish or sanding between coats.
    Thank you in advance for your kindness and I also congratulate you for the articles you wrote :). All the best.

    • Good evening.
      It would be good if you treated the wood before fitting against insects and mould. There are water-based solutions that can be applied with a brush and after drying you can apply any kind of finish. There is also ready-treated wood, but it is more expensive.
      The finishing steps are bait, primer and varnish.The bait is applied to stain the wood and can be solvent or water based. After drying, any kind of finish can be applied on top. Water-based wood stain is odourless, but dries a little harder and lifts the wood grain. Solvent-based wood stain is odorous, but the grain lifts less and sanding is easier.
      After the bath has dried, without sanding, the primer is applied. The primer is so made that it adheres well to the substrate, is thick (it has a larger solid body than varnish) and grinds very well. Apply 1-2 coats. After complete drying it is sanded. Sanding is done with 280 or 320 grit sandpaper if the lacquer to be applied is matt and over 400 if it is glossy.
      At the end apply the varnish. The varnish is formulated to be hard, scratch and abrasion resistant, aesthetically pleasing (glossy or matte, silky, etc.). In general, only one coat of varnish is applied. If a second coat has to be applied, it is applied without sanding, before the first coat is completely dry (after 30-45 min.). That way it has adhesion to the lower coat. Avoid sanding the varnish because, being made to be scratch resistant, sanding is very difficult.
      There are also products made specifically for DIY application that are a kind of primer-lacquer. These can be applied after bathing, 2-3 coats, with sanding in between, without the need for primer.
      Floor products can be water-based or solvent-based (polyurethane, acid-hardening). Hand-applied ones are approximately equal in strength. If you want a glossy finish, solvent-based ones are nicer, more transparent.
      I hope I've been useful.
      All the best!

      You can also find a lot of useful information in the printed Wood Magazine. This year there are 2 issues, in March and September. Subscription details can be found here: https://revistadinlemn.ro/product/abonament-revista-din-lemn/

      • Thank you very much for your reply. I needed objective advice and it came from a professional. At the same time, I very much appreciate the fact that you answered me very, very quickly. Congratulations on what you do (rare are the people who are so benevolent in telling of the "secrets of the trade"). Since we are celebrating this year the 100th anniversary of the Great Union, I congratulate you for being a true Romanian 🙂